Material Densification
Technical Publication

Optimizing HIP and printing parameters for EBM Ti-6Al-4V

The study explores HIP parameters for EBM Ti-6Al-4V to maximize material strength. Optimal conditions include a lower HIP temperature of 800°C and a higher pressure of 200 MPa, effectively eliminating internal defects while achieving the highest strength. Intentionally inducing porosity during printing, along with an optimized HIP cycle, further enhances material strength.

Share:

Related content

Technical Publication
Hot isostatic pressing of 3D printed alumina-toughened zirconia
Technical Publication
Mapping contributions of defects to the fatigue life of Ti6Al4V from laser powder bed fusion using quantitative fractograph
Webinar
Quintus Purus® Standard: Redefining clean HIP for critical applications
Customer Stories
MTC Powder Solutions expands PM-HIP capabilities with Quintus QIH 286
Webinar
Hot Isostatic Pressing (HIP) for Metal AM
White paper
Reducing heat treatment distortion through High Pressure Heat Treatment (HPHT™)

Need help choosing the right press for your business?