The study explores HIP parameters for EBM Ti-6Al-4V to maximize material strength. Optimal conditions include a lower HIP temperature of 800°C and a higher pressure of 200 MPa, effectively eliminating internal defects while achieving the highest strength. Intentionally inducing porosity during printing, along with an optimized HIP cycle, further enhances material strength.

Share:

Related content

Jim Shipley from Quintus Technologies and Magnus Bergman from VBN Componets
Tech Talks

Wear-resistant AM Components with VBN Components

Webinar

HIP for free: Speed printing unleashed

White paper

“HIP for free”: Speed printing unleashed

Webinar

Latest developments in state-of-the-art capabilities in HIP/HPHT™ for advanced ceramics

Brochure

Isostatic Pressing for Advanced Technical Ceramics

Customer Stories

Saab Dynamics and PartnerTech Karlskoga secure continuous production with Quintus Cold Isostatic Pressing System upgrade

This site is registered on wpml.org as a development site. Switch to a production site key to remove this banner.