Material Densification
White paper

Optimizing HIP and printing parameters for EBM Ti-6Al-4V

An investigation of HIP parameters for EBM Ti-6Al-4V has been performed by Arcam AB and Quintus Technologies AB with the aim to maximize the strength of the HIP:ed material.
Optimizing HIP and printing parameters for EBM Ti-6Al-4V

A lower HIP temperature of 800 °C and a higher pressure of 200 MPa gives the highest strength and is also enough to eliminate all internal defects. By printing material with intentionally induced porosity combined with an optimized HIP cycle the highest strength can be obtained.

Share:

Related content

White paper

Benefits of using HIP for additively manufactured thin-walled, high-performance heat exchangers

Jim Shipley from Quintus Technologies and Magnus Bergman from VBN Componets
Tech Talks

Wear-resistant AM Components with VBN Components

Webinar

HIP for free: Speed printing unleashed

White paper

HIP for free: Speed printing unleashed

Webinar

Latest developments in state-of-the-art capabilities in HIP/HPHT™ for advanced ceramics

Brochure

Isostatic Pressing for Advanced Technical Ceramics

This site is registered on wpml.org as a development site. Switch to a production site key to remove this banner.